Sanding and polishing of small defects

Sanding and polishing of small defects

Sanding:

  1. First step. Using a Mirka humidifier, apply the correct amount of abrasive fluid to the affected area.
  2. Second step. Sand the defect for 2 to 5 seconds with a "Polarstar SR5" sanding disc using a Mirka "ROS 150NV" sander.
  3. Third step. Before polishing, clean the sanded area.

Polishing:

  1. First step. Apply one drop of "Polarshine" polishing paste to the sanded surface.
  2. Second step. Polish the sanded surface for 5 to 10 seconds with a Mirka "Retic 77 x 20 mm" polishing sponge together with a Mirka "ROP2 312NV" polisher.
  3. Third step. Wipe off polishing residue with a soft microfiber cloth.